ALLOY825 (Incoloy825)
Characteristics
ALLOY825 is a titanium-stabilized fully austenitic Ni-Fe-Cr alloy with additions of Cu + Mo
- good resistance to stress-corrosion cracking
- satisfactory resistance to pitting and crevice corrosion
- good resistance to oxidizing and non-oxidizing hot acids
- good mechanical properties at both room and elevated temperatures, up to approximately 550°C (1020°F)
- approval for pressure vessels with wall temperatures up to 450°C (842°F)
Sourceable Ex-Stock Material for other Forms from Distributors World-Wide
Equivalent | Round Bars | Plate | Pipe/Tube | Welding Rod & Wire | ||
---|---|---|---|---|---|---|
Min | Max | Min | Max | |||
Incoloy825 | 6~350 | 0.81~50.8 | ○ | △ |
*○: Various sizes available in stock. △: Only limited sizes available in stock. ☆: Please contact us for more details.
* We can supply materials and products that comply with various standards including ASTM, ASME, AMS, and NACE standards. Please contact us for more details.
Corrosion resistance
Alloy 825 is a versatile general engineering alloy with resistance to corrosion in acids and alkalis under both oxidizing and reducing conditions.
High nickel content gives the alloy virtual immunity to stress corrosion cracking.
Alloy 825 is good in media as diverse as sulphuric, sulphurous, phosphoric, nitric and organic acids, alkalis such as sodium or potassium hydroxide, and acidic chloride solutions.
The versatility of Alloy 825 is illustrated by its use in nuclear fuel element dissolvers where a variety of corrosive media, e. g. sulphuric and nitric acids and sodium hydroxide, are handled in the same equipment.
Applications
Alloy 825 is used in a wide variety of applications up to a temperature of approximately 550 °C (1020 °F).
Typical applications are:
- components such as heating coils, tanks, crates, baskets and chains in sulphuric acid pickling plants
- fuel element dissolvers
- sea-water-cooled heat exchangers, offshore product piping systems; tubes and components in sour gas service
- heat exchangers, evaporators, scrubbers, dip pipes etc. in phosphoric acid production
- air-cooled heat exchangers in petroleum refineries
- food processing
- chemical plant
- combustion-resistant alloy for high pressure O2 applications
Chemical composition
Ni | Cr | Fe | C | Mn | Si | Cu | Mo | Al | Ti | P | S | |
---|---|---|---|---|---|---|---|---|---|---|---|---|
min | 38.0 | 19.5 | bal. | 1.5 | 2.5 | 0.6 | ||||||
max | 46.0 | 23.5 | 0.025 | 1.0 | 0.5 | 3.0 | 3.5 | 0.2 | 1.2 | 0.020 | 0.010 |
※The values in the table are for reference only and do not guarantee minimum or maximum values. For further information, please contact us.
Mechanical properties(Round Bar)
Condition | Yield Strength(Mpa) | Tensile Strength(Mpa) | Elongation(%) | Hardness(HB) | |
---|---|---|---|---|---|
ASTM Min Value | Soft Annealed | 241 | 586 | 30 | |
Typical Values at RT | Soft Annealed | 333 | 647 | 33 | 160 |
Please contact us with any questions about reference or value of plate and pipe.
※The values in the table are for reference only and do not guarantee minimum or maximum values. For further information, please contact us.
International Standard Comparison Chart
Material | Round Bars | Plates/Sheets | Pipe/Tube | ||
---|---|---|---|---|---|
Seamless | Welded | ||||
ASTM | UNS N08825 |
B425 | B424 | B423 | B163/704/705 |
ASME | SB425 | SB424 | SB423 | SB163 | |
JIS | NCF825 | H4553 | G4901 | H4552 | |
DIN | 2.4858 | 17752 | 17750 | 17751 |
- Disclaimer
- All the information on this website is published in good faith and for general information purpose only and not for technical design purposes. We do not make any warranties about the completeness, reliability and accuracy of this information. Any action you take upon the information on our website is strictly at your own risk. and we will not be liable for any losses and damages in connection with the use of our website.